Skip to Content

Condition Description

A part that must withstand 150 deg C continuously in strong acid sits in one of the narrowest ranges of engineering plastics selection. General-purpose materials such as PA, PC, POM and PBT are largely ruled out: either the continuous temperature rating is too low, or the material hydrolyses and stress-cracks in acid. This page lists the grades that do qualify and flags the items you need to verify.

Typical parts are chemical pump and valve components, seals, pickling jigs, exhaust duct linings and filter supports. Do not decide from the words "heat resistant" and "corrosion resistant" alone - acid type, concentration, temperature and contact time all change the answer, and hot concentrated acids always require immersion testing.

Candidate Materials for This Condition

12 products matchedAll mandatory criteria met
See excluded products (30) and reasons
  • MC浇铸尼龙板|高韧性耐疲劳|齿轮齿条传动件用Long-term temperature 115 below required 150 °C
  • MC浇铸尼龙棒|Ø6–150mm|高韧性耐磨|蜗轮轴套用Long-term temperature 115 below required 150 °C
  • PA66尼龙66板|高强度耐热|齿轮轴套通用工程塑料Long-term temperature 85 below required 150 °C
  • PA66尼龙66棒|Ø6–200mm|高强度耐磨|传动件用Long-term temperature 85 below required 150 °C
  • PA66尼龙板|90MPa高强度 低吸水0.6%|精密传动绝缘件Long-term temperature 95 below required 150 °C
  • PA66尼龙棒|90MPa高强度|精密轴套/齿轮加工用Long-term temperature 95 below required 150 °C
  • PA6尼龙板|耐磨自润滑 抗蠕变|机械结构件通用Long-term temperature 85 below required 150 °C
  • PA6尼龙棒|Ø6–200mm|耐磨抗蠕变|轴套导轨用Long-term temperature 85 below required 150 °C
  • PC/ABS合金板|高抗冲300J/M|手板模型与设备外壳Long-term temperature 90 below required 150 °C
  • PC/ABS合金棒|低温抗冲|机械零件与外壳加工Long-term temperature 90 below required 150 °C
  • PPO板(改性聚苯醚)|低介电2.65 耐热137℃|电气绝缘Long-term temperature 10 below required 150 °C
  • PPO棒|低介电高刚性|高频绝缘与化工件加工Long-term temperature 10 below required 150 °C
  • UPE980超高分子量聚乙烯板|980万分子量 极致耐磨Long-term temperature 80 below required 150 °C
  • UPE980超高分子量聚乙烯棒|980万分子量|高耐磨件Long-term temperature 80 below required 150 °C
  • 加纤PA尼龙板(GF30)|140MPa高刚性|叶轮阀体齿轮Long-term temperature 120 below required 150 °C
  • 加纤PA尼龙棒(GF30)|140MPa|高承载传动件Long-term temperature 120 below required 150 °C
  • 加纤PC板(GF30)|V-0阻燃 HDT148℃|电气结构件Long-term temperature 120 below required 150 °C
  • 加纤PC棒(GF30)|V-0阻燃 高刚性|绝缘结构件Long-term temperature 120 below required 150 °C
  • 导电PA尼龙板|10³–10⁵Ω全断面导电|半导体载具Long-term temperature 10 below required 150 °C
  • 导电PA尼龙棒|10³–10⁵Ω|防静电工装与传动件Long-term temperature 10 below required 150 °C
  • 白色PA6尼龙板|FDA食品级 色泽均匀|食品机械件Long-term temperature 85 below required 150 °C
  • 白色PA6尼龙棒|食品接触级|白色耐磨结构件Long-term temperature 85 below required 150 °C
  • 透明PC板(食品级)|FDA 177.1580|高抗冲视窗防护Long-term temperature 120 below required 150 °C
  • 透明PC棒(食品级)|高透明 抗冲800J/M|视窗与护罩Long-term temperature 120 below required 150 °C
  • 防静电PA尼龙板|10⁶–10⁹Ω|电子元件载具工装Long-term temperature 90 below required 150 °C
  • 防静电PA尼龙棒|10⁶–10⁹Ω|洁净室工装传动件Long-term temperature 90 below required 150 °C
  • 防静电PC板|透明/黑色 抗冲800J/M|洁净室视窗Long-term temperature 120 below required 150 °C
  • 防静电PC棒|高抗冲 抗静电改性|视窗与结构件Long-term temperature 120 below required 150 °C
  • 阻燃PA尼龙板|UL94 V-0|开关连接器骨架Long-term temperature 80 below required 150 °C
  • 阻燃PA尼龙棒|V-0级阻燃|电气绝缘结构件Long-term temperature 80 below required 150 °C

Your selection criteria: Long-term service temperature ≥ 150 °C · Media: Strong acids

or contact us directly

39 products match this condition. To filter by your specific parameters, use the Full Material Selector →

Basis for Judgment and Key Points

FAQ

Why are PA66 and POM unsuitable for strong acid?

PA and POM hydrolyse and stress-crack in strong acids, and their continuous temperature ratings are only around 100 deg C and 90 deg C respectively, so they fail both constraints. Glass fibre reinforcement raises strength and stiffness but does not change chemical resistance.

PEEK and PVDF are both acid resistant - which should I use?

It depends on load. PEEK has far higher strength, stiffness and creep resistance, which suits loaded structural parts, valve trim and bearings. PVDF is cheaper and suits non-load-bearing corrosion protection such as linings and piping, but its mechanical strength falls off noticeably at elevated temperature.

Do acid concentration and temperature affect the choice?

Yes, significantly. Most ratings are based on room temperature and moderate concentration; raising concentration or approaching the material temperature limit increases corrosion rate non-linearly. Verify at the worst credible combination of concentration and temperature.

Smart Material Selection