PEEK聚醚醚酮板|耐250℃ 耐化学|半导体医疗用
100% match- Long-term temperature 250 exceeds your 150 °C requirement
- Resists Strong acids ✓
Item-by-item check against your criteria
| Long-term Working Temperature | 250 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
Few materials survive 150 deg C continuous service in strong acid. This page lists the candidates - PEEK, PVDF, PPS, PTFE - with their strength, creep and cost trade-offs.
A part that must withstand 150 deg C continuously in strong acid sits in one of the narrowest ranges of engineering plastics selection. General-purpose materials such as PA, PC, POM and PBT are largely ruled out: either the continuous temperature rating is too low, or the material hydrolyses and stress-cracks in acid. This page lists the grades that do qualify and flags the items you need to verify.
Typical parts are chemical pump and valve components, seals, pickling jigs, exhaust duct linings and filter supports. Do not decide from the words "heat resistant" and "corrosion resistant" alone - acid type, concentration, temperature and contact time all change the answer, and hot concentrated acids always require immersion testing.
| Long-term Working Temperature | 250 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 250 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 170 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 170 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 160 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 160 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 220 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 220 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 160 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 160 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 150 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
| Long-term Working Temperature | 150 | ✓ |
|---|---|---|
| Strong acids resistance | Good (+) | ✓ |
Your selection criteria: Long-term service temperature ≥ 150 °C · Media: Strong acids
or contact us directly39 products match this condition. To filter by your specific parameters, use the Full Material Selector →
PA and POM hydrolyse and stress-crack in strong acids, and their continuous temperature ratings are only around 100 deg C and 90 deg C respectively, so they fail both constraints. Glass fibre reinforcement raises strength and stiffness but does not change chemical resistance.
It depends on load. PEEK has far higher strength, stiffness and creep resistance, which suits loaded structural parts, valve trim and bearings. PVDF is cheaper and suits non-load-bearing corrosion protection such as linings and piping, but its mechanical strength falls off noticeably at elevated temperature.
Yes, significantly. Most ratings are based on room temperature and moderate concentration; raising concentration or approaching the material temperature limit increases corrosion rate non-linearly. Verify at the worst credible combination of concentration and temperature.