MC浇铸尼龙板|高韧性耐疲劳|齿轮齿条传动件用
100% match- Tensile Strength excels: 75
Item-by-item check against your criteria
| Long-term Working Temperature | 115 | — |
|---|---|---|
| Tensile Strength | 75 | ✓ |
Precision fits fail through moisture growth, not strength. Ranked by dimensional stability and creep, this page lists POM, PEEK and PC candidates and quantifies PA moisture growth.
Precision fits (IT7 and tighter) in engineering plastics rarely fail because of insufficient strength; they fail because dimensions drift with ambient humidity. PA nylon is the usual culprit: equilibrium moisture absorption is typically 1.5 to 2.5 percent, producing dimensional change of 0.3 to 0.6 percent - enough to consume the entire fit tolerance.
This page ranks candidates by dimensional stability, creep resistance and strength. POM absorbs about 0.2 percent moisture, has good stiffness and machines stably, making it the default for precision parts; PEEK balances temperature resistance and dimensional stability at higher cost; PC is dimensionally stable and tough, but only average in chemical and wear resistance.
| Long-term Working Temperature | 115 | — |
|---|---|---|
| Tensile Strength | 75 | ✓ |
| Long-term Working Temperature | 115 | — |
|---|---|---|
| Tensile Strength | 75 | ✓ |
| Long-term Working Temperature | 85 | — |
|---|---|---|
| Tensile Strength | 74 | ✓ |
| Long-term Working Temperature | 85 | — |
|---|---|---|
| Tensile Strength | 74 | ✓ |
| Long-term Working Temperature | 95 | — |
|---|---|---|
| Tensile Strength | 90 | ✓ |
| Long-term Working Temperature | 95 | — |
|---|---|---|
| Tensile Strength | 90 | ✓ |
| Long-term Working Temperature | 85 | — |
|---|---|---|
| Tensile Strength | 74 | ✓ |
| Long-term Working Temperature | 85 | — |
|---|---|---|
| Tensile Strength | 74 | ✓ |
| Long-term Working Temperature | N/A | — |
|---|---|---|
| Tensile Strength | 80 | ✓ |
| Long-term Working Temperature | N/A | — |
|---|---|---|
| Tensile Strength | 80 | ✓ |
| Long-term Working Temperature | 250 | — |
|---|---|---|
| Tensile Strength | 95 | ✓ |
| Long-term Working Temperature | 250 | — |
|---|---|---|
| Tensile Strength | 95 | ✓ |
Your selection criteria: Tensile strength ≥ 60 MPa
or contact us directly56 products match this condition. To filter by your specific parameters, use the Full Material Selector →
Conditioning brings parts close to the moisture equilibrium of the service environment quickly and reduces further growth, but it does not remove the effect of humidity fluctuation itself. Where humidity varies widely, tolerance the part for the wettest condition.
Choose POM for ambient temperature, ordinary media and cost sensitivity; choose PEEK where high temperature, chemical resistance or longer life is required. POM machines well and holds dimensions, which is why it is the most common precision-part material.
It depends on material, wall thickness and process. Machined POM and PEEK commonly reach plus or minus 0.05 mm, tighter with special design; injection moulded parts are governed by shrinkage and tooling, so tolerances follow the material shrinkage. Moisture-absorbing materials should be dimensioned in the conditioned state.